FeCoNiCrTi High-Entropy Alloy (HEA) Spherical Powder is usually created using a powder metallurgy technique, which facilitates meticulous control over both its composition and the size of its particles. Stanford Advanced Materials (SAM) possesses extensive expertise in the production and provision of top-grade Fe-based Alloy Spherical Powder.
Related products: Spherical Bronze Alloy Powder CuSn10, CuCrZr High-Entropy Alloy (HEA) Spherical Powder, Copper Chromium Nanopowder, CuCr
FeCoNiCrTi High-Entropy Alloy (HEA) Spherical Powder is usually created using a powder metallurgy technique, which facilitates meticulous control over both its composition and the size of its particles. Stanford Advanced Materials (SAM) possesses extensive expertise in the production and provision of top-grade Fe-based Alloy Spherical Powder.
Related products: Spherical Bronze Alloy Powder CuSn10, CuCrZr High-Entropy Alloy (HEA) Spherical Powder, Copper Chromium Nanopowder, CuCr
FeCoNiCrTi High-Entropy Alloy (HEA) Spherical Powder is a sophisticated alloy comprising iron (Fe), cobalt (Co), nickel (Ni), chromium (Cr), and titanium (Ti). This alloy is part of the high-entropy alloys (HEAs) family, a relatively recent category of materials known for their distinct properties. HEAs stand out for their remarkable strength, hardness, and enhanced resistance to wear and corrosion.
The production of FeCoNiCrTi powder is typically carried out through powder metallurgy processes, ensuring precise control of its composition and particle size. This high-performance alloy demonstrates excellent mechanical properties and corrosion resistance, especially at high temperatures. Iron and cobalt contribute significantly to its high-temperature strength, nickel adds to its ductility and toughness, and chromium offers superior oxidation and corrosion resistance.
Density |
8.0-8.5 g/cm3 |
Melting Point |
1300-1400℃ |
Thermal Conductivity |
10-30 W/mK |
Electrical Resistivity |
70-90 μΩ.cm |
Young’s Modulus |
180-220 GPa |
Poisson’s Ratio |
0.28-0.32 |
Tensile Strength |
650-1100 MPa |
Yield Strength |
450-750 MPa |
Elongation |
10-30% |
Hardness |
25-50 HRC |
Chemical Composition (%)
Iron (Fe) |
Balance |
Cobalt (Co) |
35-50% |
Nickel (Ni) |
10-30% |
Chromium (Cr) |
8-12% |
Titanium (Ti) |
0.5-2% |
Carbon (C) |
0.5% max |
Silicon (Si) |
1% max |
Manganese (Mn) |
1% max |
Our FeCoNiCrTi High-Entropy Alloy (HEA) Spherical Powder is carefully handled during storage and transportation to preserve the quality of our product in its original condition.