Spherical Cobalt Based Alloy Powder Co6 is produced by advanced gas atomization and water atomization. Stanford Advanced Materials (SAM) has rich experience in manufacturing and supplying high-quality Spherical Cobalt Based Alloy Powder Co6.
Related products: Ti-8Mn Titanium Alloy Spherical Powder, Ti-17 Titanium Alloy Spherical Powder, Ti Grade 12 Titanium Alloy Spherical Powder
Spherical Cobalt Based Alloy Powder Co6 is produced by advanced gas atomization and water atomization. Stanford Advanced Materials (SAM) has rich experience in manufacturing and supplying high-quality Spherical Cobalt Based Alloy Powder Co6.
Related products: Ti-8Mn Titanium Alloy Spherical Powder, Ti-17 Titanium Alloy Spherical Powder, Ti Grade 12 Titanium Alloy Spherical Powder
Spherical Cobalt Based Alloy Powder Co6 is produced by advanced gas atomization and water atomization. The alloy powder features low oxygen content, and high sphericity, and uniform particle size.
Cobalt Based Alloy Powder is widely used in high-temperature and high-pressure valves, valve seats, engine valves, internal combustion engines, inlet/outlet valves, gardening tools, turbine blades, bearings and hot cutting edges, etc.
Chemical Composition (%)
Grade |
C |
Cr |
Si |
W |
Ni |
Fe |
Mn |
Mo |
Co |
Co 1 |
2.5 |
30 |
1 |
12.0 |
≤3.0 |
≤3.0 |
≤1.0 |
≤1.0 |
Bal |
Co 6 |
1.2 |
30 |
1 |
4.5 |
≤3 |
≤3 |
≤1.0 |
≤1.0 |
Bal. |
Co 12 |
1.4 |
30 |
1.4 |
8.5 |
≤3 |
≤3 |
≤1.0 |
≤1.0 |
Bal. |
Co 21 |
0.2 |
28 |
2 |
0.15 |
≤3 |
2 |
≤1.0 |
5.5 |
Bal. |
Physical properties
Flow Density (g/cm3) |
4.3-4.8 |
Size (μm) |
15-53 |
Hardness |
38 HRC |
Production process |
Gas atomized |
Our Spherical Cobalt Based Alloy Powder Co6 is carefully handled during storage and transportation to preserve the quality of our product in its original condition.