Lithium Cobalt Oxide Cathode Material (LCO Powder) is now widely used as the cathode material of choice in rechargeable lithium-ion batteries found in consumer electronics products. Stanford Advanced Materials (SAM) has rich experience in manufacturing and supplying high-quality Lithium Cobalt Oxide Cathode Material (LCO Powder).
Related products: Lithium Iron Phosphate Powder LiFePO4, LFP, Lithium Cobalt (III) Oxide Powder (LCO Powder), Lithium Manganese Oxide Powder (LMO Powder)
Lithium Cobalt Oxide Cathode Material (LCO Powder) is now widely used as the cathode material of choice in rechargeable lithium-ion batteries found in consumer electronics products. Stanford Advanced Materials (SAM) has rich experience in manufacturing and supplying high-quality Lithium Cobalt Oxide Cathode Material (LCO Powder).
Related products: Lithium Iron Phosphate Powder LiFePO4, LFP, Lithium Cobalt (III) Oxide Powder (LCO Powder), Lithium Manganese Oxide Powder (LMO Powder)
Lithium Cobalt Oxide Cathode Material (LCO Powder) is a 4.4V high-energy density LCO cathode material, which is suitable for high-end 3C lithium-ion batteries. This product not only has a superior cycle performance in normal temperature but also adapt well in ultra-high and low-temperature environment.
CAS Number |
12190-79-3 |
Appearance |
Black powder |
Molecular Formula |
LiCoO2 |
Purity |
>99.5% |
Formula Weight |
97.88 g/mol |
Synonym |
Lithium Cobaltite |
Chemical Name or Material |
Lithium Cobalt (III) Oxide |
Particle Size (D10) |
≥4.0 µm |
Particle Size (D50) |
14.0~18.0 µm |
Particle Size (D90) |
≤45.0 µm |
TAP density |
≥2.4 g/cm3 |
BET Specific Surface Area |
0.10 ~ 0.30 m2/g |
pH |
≤10.8 |
Discharge Capacity (mAh/g) |
≥188 (typical 190.6) @0.1 C; ≥175 (typical 180.2) @1 C. (vs. Li, 0.1 C, 3.0~ 4.5 V, coin cell) |
Efficiency |
≥95% @0.1 C. (vs. Li, 0.1 C, 3.0~4.5 V, coin cell) |
Chemical Analysis |
wt% |
Li |
7.0±0.5 |
Co |
59.0~61.0 |
Na |
≤0.02 |
Ca |
≤0.02 |
K |
≤0.01 |
Cr |
≤0.005 |
Cd |
≤0.005 |
Pb |
≤0.001 |
Cu |
≤0.005 |
Fe |
≤0.015 |
Mn |
≤0.02 |
Moisture |
≤0.10 |
Residual Li2CO3 |
≤0.06 |
Lithium Cobalt Oxide Cathode Material (LCO Powder) is widely used as the cathode material of choice in rechargeable lithium-ion batteries found in consumer electronics products.
Our Lithium Cobalt Oxide Cathode Material (LCO Powder) is carefully handled during storage and transportation to preserve the quality of our product in its original condition.